The determining method is described as follows:12 samples of 3mm X 4mm X 36mm in 99.5% ceramic,99% ceramic or 95% ceramic are put into the furance and are heated to 200 ÂșC and kept for 30 minutes and then are put into the flowing water with common temperature and the samples should not be cracked.